Everything engineers and procurement managers need to specify compliant brass: RoHS 2011/65/EU, REACH SVHC, ISO 6509-1 DZR, EN product standards, and global potable water approvals (WRAS, KIWA, ACS, DVGW, NSF 61) — checked directly against publishing standards.
2011/65/EU · Lead exemption 6(c) · June 2027 deadline
SVHC candidate list · Article 33 duty · Lead in brass
Dezincification resistance · test method · alloy qualification
EN 12164 · EN 12165 · EN 12167 · EN 12168
WRAS · KIWA · ACS · DVGW · NSF 61
13 key grades vs. every standard at a glance
The Restriction of Hazardous Substances Directive limits lead to ≤0.10% by weight in electrical and electronic equipment (EEE). Leaded brass alloys exceed this limit and rely on a critical exemption.
RoHS 2 (2011/65/EU, amended by 2015/863/EU) restricts 10 hazardous substances in EEE sold in the EU. For brass, the critical substance is lead (Pb), restricted to a maximum of 0.10% by weight in homogeneous materials.
Leaded brass alloys (CW617N, CW614N, CW625N, CW612N, CW607N, CW603N) contain roughly 0.8–3.5% lead — far above the 0.10% threshold. They cannot be used in EEE without a specific exemption.
Key threshold: Pb ≤ 0.10% → RoHS free (no exemption required). Pb > 0.10% → must use Exemption 6(c) while it remains valid.
| Feb 2003 | Original RoHS Directive 2002/95/EC enters force |
| July 2011 | RoHS 2 (2011/65/EU) expands scope to more product categories |
| June 2018 | Exemption 6(a) granted for lead in copper alloys at ≤4% by weight |
| 30 Jun 2027 | Exemption 6(c) current expiry — renewal required or switch to lead-free grades |
Annex III, Exemption 6(c) of RoHS 2 permits the use of lead as an alloying element in copper alloys, containing up to 4% lead by weight in EEE components.
Official text: “Lead as an alloying element in copper with a lead content up to 4% by weight”
Exemption 6(c) has been renewed multiple times — most recently by Commission Delegated Directive (EU) 2024/2304. The current validity expires 30 June 2027.
Six alloys in our portfolio carry Pb ≤ 0.10% and require no RoHS exemption:
| ALLOY | FAMILY | LEAD CONTENT (PB) | ROHS STATUS |
|---|---|---|---|
| CW724RCuZn21Si3P | Silicon Brass | ≤ 0.10% | ✓ RoHS free — no exemption needed |
| C6802JIS H3250 | Bismuth Brass | ≤ 0.10% | ✓ RoHS free — no exemption needed |
| CW614NCuZn39Pb3 | Free-machining | 2.5–3.5% | Requires Exemption 6(c) |
| CW617NCuZn40Pb2 | Forging / machining | 1.6–2.5% | Requires Exemption 6(c) |
| CW602NCuZn36Pb2As | DZR Brass | 1.7–2.8% | Requires Exemption 6(c) |
REACH regulates chemicals manufactured or imported into the European Union. Unlike RoHS, REACH does not ban lead outright in brass — it requires communication across the supply chain under Article 33.
In June 2018, the European Chemicals Agency (ECHA) added lead metal (EC 231-100-4, CAS 7439-92-1) to the Candidate List of Substances of Very High Concern (SVHC) due to its toxic-for-reproduction properties.
Because brass contains lead above the 0.10% w/w threshold, manufacturers and suppliers of brass articles have specific legal duties under REACH Article 33:
Any supplier of an article containing lead > 0.1% must provide the recipient with sufficient information to allow safe use of the article — at minimum, the name of the substance (Lead, CAS 7439-92-1).
Under the Waste Framework Directive, companies supplying articles containing SVHCs > 0.1% to the EU must submit notification data to ECHA’s SCIP database before placing on the market.
| FEATURE | ROHS | REACH |
|---|---|---|
| Scope | Electrical equipment | All articles & mixtures |
| Mechanism | Substance ban (≤0.1% Pb) | Notification (>0.1% Pb) |
| Exemption | Exemption 6(c) (≤4% Pb) | No exemption — declare |
| Lead-free | No exemption needed | No declaration needed |
Inform customers if lead is present > 0.1%. Standard Mihir Enterprise material test reports declare lead content precisely to fulfill Article 33 duties.
EU importers and assemblers must submit data to the ECHA SCIP database for parts containing > 0.1% lead by weight.
Lead in brass is not currently subject to Annex XIV authorization, but entry 63 of Annex XVII restricts lead in consumer jewellery and articles accessible to children.
Dezincification is a selective corrosion mechanism that leaches zinc from brass in water contact, leaving a porous, mechanically weak copper matrix. ISO 6509-1 is the internationally recognized benchmark test method.
In duplex brasses (α+β phase, zinc > 35%), the zinc-rich beta phase corrodes preferentially. Over time, zinc ions dissolve into warm, stagnant, or acidic water, leaving behind weak, brittle copper that causes fitting leaks and wall fractures.
Layer-type attack: uniform thinning across large surface areas in soft, acidic waters.
Plug-type attack: localized deep penetration in neutral or alkaline waters at elevated temperatures, penetrating walls rapidly.
Inhibited alloys use small additions of arsenic (0.02–0.15% As in CW602N) or silicon (2.7–3.5% Si in CW724R) together with specialized heat treatment to inhibit the corrosion reaction.
1.0% cupric chloride solution (CuCl2 · 2H2O)
75 ± 2 °C for 24 continuous hours
Maximum dezincification depth ≤ 100 μm (or ≤ 200 μm per regional specs)
CW602N (CuZn36Pb2As): Arsenic inhibits redeposition of copper, provided proper annealing dissolves beta phase into alpha.
CW724R / C69300: Intrinsic DZR by alloy composition. Forms a protective kappa-phase barrier without needing arsenic.
Strict post-machining or post-forging stress-relief and annealing cycles ensure phase equilibrium and prevent intergranular corrosion.
European Norm (EN) standards define the compositional limits, mechanical properties, and quality requirements for brass wrought products. These are the standards referenced in Mihir Enterprise’s material certifications.
Primary standard for free-machining brass rods (CW614N, CW617N, CW602N, CW724R) turned on automatic screw machines and CNC lathes.
Defines extruded rod and cast billets intended for hot stamping and die pressing (CW617N, CW602N).
Covers architectural extrusions, custom sectional profiles, and seamless hollow bars for weight and machining optimization.
Statement of compliance with order without test results.
Test results from general manufacturing quality control.
Actual heat chemical analysis (optical emission spectrometer) and mechanical test data from the supplied batch.
Mihir Enterprise supplies EN 10204 Type 3.1 certificates as standard on all machined component shipments.
Fittings and components in contact with drinking water are approved under national or regional rules. In Europe, metals are accepted by listed composition; NSF/ANSI 61 tests leaching from the finished product. The approval always belongs to the finished product.
Regulatory concern about lead in drinking water has grown since the 2010s. The WHO guideline value is 10 μg/L, and EU Drinking Water Directive (EU) 2020/2184 lowers the EU limit from 10 to 5 μg/L by January 2036 — markets are moving toward low-lead and lead-free alloys for potable-water contact.
In the US, leaded brasses such as CW617N (Pb 1.6–2.2%) are above the 0.25% weighted-average lead limit of NSF/ANSI 372 for wetted parts. In the EU, the European positive list that applies from 31 December 2026 contains no leaded brass; national approvals remain usable until 31 December 2032. The lead-free grades CW724R (silicon brass) and C6802 (bismuth brass) stay within the US limit, and CW724R is on the European positive list.
A listed alloy is necessary but not sufficient — the approval (WRAS, Kiwa, ACS, DVGW, NSF/ANSI 61) is granted to the finished component.
Voluntary evidence that a fitting complies with Regulation 4 of the Water Supply Regulations 1999. BS 6920 tests non-metallic parts for water quality effects.
WRAS listings are searchable at wrasapprovals.co.uk.
Products meet the Drinkwaterbesluit and Regeling materialen en chemicaliën. Quality declaration certificate issued by Kiwa Nederland.
Until full EU system is active, Dutch system rests on 4MS common approaches.
French sanitary conformity attestation under Arrêté of 29 May 1997 for contact with human drinking water.
A purely metallic part needs no ACS of its own — its alloy must be on the accepted list.
German technical & scientific association certifying drinking water products. Metallic materials are assessed against the Umweltbundesamt (UBA) list of accepted alloys.
For a brass part, the key question is whether its alloy is on the UBA list for its product group.
Covers health effects — leaching of metals into potable water. NSF/ANSI 372 requires a weighted average lead content ≤0.25% across all wetted surfaces.
C6802, CW724R, and C69300 have lead limits ≤0.10%, well inside the 0.25% statutory figure.
Thirteen of our most-specified alloys, mapped against RoHS, REACH, dezincification resistance, the EN product standard and the lead rules for drinking water. See the full materials library for all 30 grades.
| ALLOY | ROHS | REACH ART. 33 | DZR (ISO 6509-1) | EN TITLE | US LEAD (NSF 372) | EU POSITIVE LIST |
|---|---|---|---|---|---|---|
| CW617NCuZn40Pb2 | 6(c) | SVHC > 0.1% | × No | ✓ 12164 | × Pb 1.6–2.2% | National only * |
| CW614NCuZn39Pb3 | 6(c) | SVHC > 0.1% | × No | ✓ 12164 | × Pb 2.5–3.5% | National only * |
| CW602NCuZn36Pb2As | 6(c) | SVHC > 0.1% | ✓ DZR | ✓ 12164 | × Pb 1.7–2.8% | National only * · 2032 |
| CW612NCuZn39Pb2 | 6(c) | SVHC > 0.1% | × No | ✓ 12164 | × Pb 1.8–2.5% | National only * |
| CW607NCuZn38Pb1 | 6(c) | SVHC > 0.1% | × No | ✓ 12164 | × Pb 0.8–1.6% | National only * |
| CW603NCuZn36Pb3 | 6(c) | SVHC > 0.1% | ✓ DZR | ✓ 12164 | × Pb 1.5–2.5% | National only * |
| CW724RCuZn21Si3P | ✓ RoHS Free | Not regulated | ✓ DZR | ✓ 12164 | ✓ Pb ≤ 0.10% | ✓ Positive list · B, C |
| C6802JIS H3250 | ✓ RoHS Free | Not regulated | × No | JIS H3250 | ✓ Pb ≤ 0.10% | Evaluating * |
| CuZn21EN 12167 | ✓ RoHS Free | Not regulated | × No | EN 12167 | ✓ Pb ≤ 0.05% | ✓ Positive list |
| CuZn40EN 12167 | Exemption 6(c) | SVHC if >0.1% | × No | EN 12167 | ✓ Pb ≤ 0.20% | ✓ Positive list |
| CW510LEN 12167 | Exemption 6(c) | SVHC if >0.1% | × No | EN 12167 | ✓ Pb ≤ 0.20% | ✓ Positive list |
| C27450UNS C27450 | 6(c) | SVHC if >0.1% | × No | ASTM B371 | ✓ Pb ≤ 0.25% | Evaluating * |
| C11000ETP Copper | ✓ RoHS Free | Not regulated | N/A (Cu) | EN 13601 | ✓ No lead added | ✓ Cu-ETP Positive |
The common ones are ISO 6509-1 (dezincification), EN 12164 / 12165 / 12420 (rod, forging stock and dimensions), the EN product standards for valves and fittings, plus regulatory rules — RoHS 2011/65/EU, REACH EC 1907/2006, and potable approvals (WRAS, NSF/ANSI 61, the EU Drinking Water Directive).
Brass used in electrical and electronic equipment falls under RoHS; the lead in copper alloy exemption 6(c) has historically permitted leaded brass, but with the exemption under review, lead-free grades are increasingly specified.
REACH Article 33 requires suppliers to inform customers when an article contains a Substance of Very High Concern above 0.1%. Lead in leaded brass is an SVHC, so a declaration is provided to downstream users.
ISO 6509-1 is the test method; a grade marked DZR/CR (for example CW602N) with a passing ISO 6509-1 result and an EN 10204 3.1 mill certificate demonstrates resistance.
Every regulatory date, test method, and threshold on this page is taken from the publishing body. Open the official source to verify any claim.
From RoHS-free silicon brass to DZR alloys tested to ISO 6509-1 — tell us your market and application, and we’ll supply the right grade with an EN 10204 3.1 mill certificate on every shipment.
Full datasheets for all 30 brass and copper alloys with chemical composition, mechanical properties, and machinability data.
Industry-specific guidance: Plumbing, Electrical, Automotive, HVAC, Industrial, and Renewable Energy applications.
CNC machining, Swiss turning, and hot forging — process parameters, tolerances, and alloy selection guidance.
Mihir Enterprise manufactures brass turned parts and CNC machined components to your drawing in Jamnagar, India, including precision turned brass components on 30+ Swiss-type lathes, with an EN 10204 3.1 certificate on every shipment.
Dedicated reference pages with full value tables, diagrams and honest limits — one standard per page.
2.1 · 2.2 · 3.1 · 3.2 — who signs what
Full f/m/c/v + H/K/L value tables
The standard behind every turned part
1% CuCl2 · 75°C · 24 h — explained
Blank → forge → EN 12420 → machining
Every brass on the list, lead limits, EU status
Every DIN, ISO, EN, ASTM & SAE page — A to Z